| Specification |
Classification: Graphitized Composites;
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Abrasion Resistance, Thermal Shock Resistance;
Usage: Aerospace, Automotive Manufacturing, Electronic Equipment, High-Temperature Furnaces;
Purity(%): ≥99.0;
Ash Content(%): <0.1;
Bulk Density(g/cm3): ≥1.72;
Apparent Porosity(%): <15;
Resistivity(μω-M): ≤10;
Cold Modulus of Rapture(MPa): 15-25;
Max Working Temperature(℃): ≥2800;
|
Feature: Long Time Materials, Instant Materials;
Product Name: Thermal Analysis Carbon Cup;
Temperature Range: 1250-1370;
Carbon Equivalen: 3.2%-4.8%;
Carbon Content: 2.3%-4.2%;
Silicon Content: 0.6%-3.8%;
Types: Round and Square Type;
Measurement Function: Thermal Analysis Towards Cast Iron;
Measuring Time: 240 Seconds at Most;
Refractoriness (℃): 1580< Refractoriness< 1770;
Type: Refractory Material;
|
Feature: Long Time Materials, Instant Materials;
Shape: Powder;
Product Name: Thermal Analysis Carbon Cup;
Temperature Range: 1250-1370;
Carbon Equivalen: 3.2%-4.8%;
Carbon Content: 2.3%-4.2%;
Silicon Content: 0.6%-3.8%;
Types: Round and Square Type;
Measurement Function: Thermal Analysis Towards Cast Iron;
Measuring Time: 240 Seconds at Most;
Refractoriness (℃): 1770< Refractoriness< 2000;
Type: Heat-Resistant Material;
Material: Silicon Carbide (SiC);
|
Feature: Long Time Materials, Instant Materials;
Shape: Block;
Product Name: Thermal Analysis Carbon Cup;
Temperature Range: 1250-1370;
Carbon Equivalen: 3.2%-4.8%;
Carbon Content: 2.3%-4.2%;
Silicon Content: 0.6%-3.8%;
Types: Round and Square Type;
Measurement Function: Thermal Analysis Towards Cast Iron;
Measuring Time: 240 Seconds at Most;
Refractoriness (℃): Refractoriness> 2000;
Type: Magnesium Oxide Boards;
Material: Alumina Cement;
|
Feature: Long Time Materials, Instant Materials;
Product Name: Thermal Analysis Carbon Cup;
Temperature Range: 1250-1370;
Carbon Equivalen: 3.2%-4.8%;
Carbon Content: 2.3%-4.2%;
Silicon Content: 0.6%-3.8%;
Types: Round/Square;
Measurement Function: Thermal Analysis Towards Cast Iron;
Measuring Time: 240 Seconds at Most;
Refractoriness (℃): 1580< Refractoriness< 1770;
Type: Refractory Material;
|