| Specification |
Color: Black, Blue, Grey, Red, Transparent, White, Yellow;
After-sales Service: 10 Years;
Warranty: 10 Years;
Material: Acrylic;
Kind: Transparent Plastic Sheet;
Water Absorption: <0.01%;
Contraction Percentage: <0.4%;
Tensile Strength: 51~80MPa;
Raw Material: 100% Virgin MMA;
Density: 1.2g/cm3;
Transmittance: 94%;
Acrylic Product Category: Transparent Color Frosted Pattern Marble Mirror;
Standard Size: Customization (1220X2440, 2050X3050, 1220X1830;
Thickness: 1.8mm 2mm 3mm 5mm 6mm 8mm 10mm 12mm 18mm 20mm 25mm;
Customized: Size and Colour Can Customized;
Performance: Flexible, Eco-Friendly, Recyclable, Durable, Smoot;
Features: UV Resistant, Flame Retardant , Waterproof;
Peculiarity: Cutting Without Odor, Bending Without Cracking;
Jinbao Factory Strength: 35 Production Line, 7-10 Days Delivery;
Other Name: PMMA Sheet, Acrilico Sheet;
Application: Advertising, Sign, Furniture, Crafts, Bathtub;
|
Material: PVC;
Kind: PVC Plastic Sheet;
Water Absorption: No;
Contraction Percentage: 0.4%~1.4%;
Tensile Strength: 3.6MPa;
Color: White;
Thickness: 1-25mm;
Density: 0.3-0.8g/cm3;
Packing: Plastic Bags;
MOQ: 2000kg;
Payment: LC Tt;
Application: Advertising, Furniture etc;
|
After-sales Service: 24 Hours;
Warranty: 24 Hours;
Material: PP;
Kind: Hard Plastic Sheet;
Water Absorption: <0.01%;
Contraction Percentage: 1.0%~2.5%;
Tensile Strength: 41~50MPa;
Color: Natural, Grey (Ral7032), Black, Light Blue, Yellow;
Length: Customized;
Size: Customized;
Surface: Glossy, Embossed or Customized;
|
Delivery: 2-7 Days;
Size: Standard;
Style: Customized;
Packing: Woven Bags;
Advantage: Environmental-Friedly,Nontoxic;
Hardness Shore C: 15-35;
Tensile: >3 MPa;
Elongation: >120%;
Tearing Strength: 260n/M;
Compression Strength: >30+/-10kpa;
Dimensional Change: <3.2%;
Thermal Conductivity: <0.038W/M.K;
Absorbent: <0.04kg/Cm2;
Burning Speed: 50 mm/Min;
|
Delivery: 2-7 Days;
Size: Standard;
Style: Customized;
Packing: Woven Bags;
Advantage: Environmental-Friedly,Nontoxic;
Hardness Shore C: 15-35;
Tensile: >3 MPa;
Elongation: >120%;
Tearing Strength: 260n/M;
Compression Strength: >30+/-10kpa;
Dimensional Change: <3.2%;
Thermal Conductivity: <0.038W/M.K;
Absorbent: <0.04kg/Cm2;
Burning Speed: 50 mm/Min;
|